We always continually provide you with the most conscientious customer service, and the widest variety of designs and styles with finest materials. These efforts include the availability of customized designs with speed and dispatch for Glass Insulation Coating, Waterborne Pigment, Types Of Dyes And Pigments, Safety as a result of innovation is our promise to each other.
Hot sale Absorbs Infrared Radiation - PSA/UV Resin Specific Heat Insulation Medium – Huzheng Detail:

Product Series

No. Code Appearance Solid content% Haze of coating film% VLT+IRR % VLT %
1 CQ-81G16-TOL Black blue liquid 16 1.50 VLT+IRR≥ 165 70
2 6JH-81L30-TOL Black blue liquid 30 0.5 VLT+IRR≥ 169 70
3 CQS-81G16-TOL Black liquid 15 0.75 VLT+IRR≥ 145 50

Product Feature
Good versatility, good compatibility, can match with most PSA or UV resin;
High heat insulation rate, the blocking rate of UV and IR is over 99%;
A number of independent intellectual property rights support, small dosage, cost-effective;
Strong weather resistance, after QUV 5000h test, no performance degradation, no color change;
Safe and reliable, no toxic and hazardous substances such as halogen, heavy metal, etc.

Product Application
It can be used in PSA or UV resin, for window film such as building window film, automotive solar film, or other fields that has the requirement of infrared blocking.

Application Method
Note: Small sample test with resin is necessary before use.
Take using in PSA resin for example, the detailed application steps are as follows:
First step: Taking out the below material by weight ratio: GTO solution: diluting agent: PSA resin=1:4:4. Adjusting the GTO dosage according to the parameter requested (7490) with testing machine with 950nm.
Diluting agent: the mixing of EA:TOL =1:1
Second step: Mixing. Mix them one by one: adding GTO solution — adding diluting agent — stirring — adding PSA resin while stirring. Stirring for about 40min after adding PSA, and then filtering the mixture with 1um filter cloth.
Third step: Choosing PET basic film. Choose the PET basic film with VLT over 90% and corona layer.
Fourth step: Coating. Coat them (the mixture in step 2) on the PET film by wet film coating machine.
Fifth step: Drying, laminating. Controlling the coating thickness between 6-8um, drying Temperature: 85~120 deg.

Package & Storage
Packing: 20 kgs/barrel.
Storage: in a cool, dry place, avoiding sun exposure.


Product detail pictures:

Hot sale Absorbs Infrared Radiation - PSA/UV Resin Specific Heat Insulation Medium – Huzheng detail pictures


Related Product Guide:
Copper nanoparticle Highly effective antibacterial

Our organization insists all along the quality policy of "product quality is base of business survival; purchaser gratification is the staring point and ending of an business; persistent improvement is eternal pursuit of staff" as well as the consistent purpose of "reputation 1st, purchaser first" for Hot sale Absorbs Infrared Radiation - PSA/UV Resin Specific Heat Insulation Medium – Huzheng , The product will supply to all over the world, such as: Montreal, USA, Korea, We integrate all our advantages to continuously innovate, improve and optimize our industrial structure and product performance. We will always believe in and work on it. Welcome to join us to promote green light, together we will make a better Future!
  • We always believe that the details decides the company's product quality, in this respect, the company conform our requirements and the goods are meet our expectations.
    5 Stars By Heather from Maldives - 2017.10.27 12:12
    It is not easy to find such a professional and responsible provider in today's time. Hope that we can maintain long-term cooperation.
    5 Stars By trameka milhouse from Tanzania - 2017.08.28 16:02
    Write your message here and send it to us